[1]狄 娜,张清芬.doi: 10.3969/j.issn.1001-3849.2025.08.008镀锌钢复合表面处理及耐腐蚀与延迟结冰性能研究[J].电镀与精饰,2025,(08):48-55.
 Di Na*,Zhang Qingfen.Research on surface treatment, corrosion resistance and delayed freezing performance of galvanized steel composite[J].Plating & Finishing,2025,(08):48-55.
点击复制

doi: 10.3969/j.issn.1001-3849.2025.08.008镀锌钢复合表面处理及耐腐蚀与延迟结冰性能研究()

《电镀与精饰》[ISSN:1001-3849/CN:12-1096/TG]

卷:
期数:
2025年08
页码:
48-55
栏目:
出版日期:
2025-08-31

文章信息/Info

Title:
Research on surface treatment, corrosion resistance and delayed freezing performance of galvanized steel composite
作者:
狄 娜1张清芬2
(1. 长春科技学院 视觉艺术学院,吉林 长春 130600 ;2. 哈尔滨工业大学 机电工程学院,黑龙江 哈尔滨 150006)
Author(s):
Di Na1* Zhang Qingfen2
(1. School of Visual Arts, Changchun Sci-Tech University, Changchun 130600, China; 2. School of Mechatronics Engineering, Harbin Institute of Technology, Harbin 150006, China)
关键词:
复合表面处理镀锌钢磷化封闭处理表面修饰延迟结冰性能
Keywords:
composite surface treatment galvanized steel phosphating sealing treatment surface finishing delayed freezing performance
分类号:
TQ153
文献标志码:
A
摘要:
通过磷化与封闭处理并结合表面修饰,在镀锌钢表面制备出具有微纳米粗糙结构并且以Zn、Ca、P、O、Ce和C元素为主要成分的超疏水涂层,其腐蚀电流密度仅为9.04×10?7 A/cm 2,能较长时间耐受中性溶液和酸碱性溶液腐蚀,相比于镀锌钢表现出更好的耐腐蚀性能。该涂层还能实现延迟结冰效果,具有良好的延迟结冰性能。通过复合表面处理可在镀锌钢表面形成具有微纳米粗糙结构和低表面能的超疏水涂层,有效阻挡腐蚀介质渗透并降低腐蚀速度,还能阻碍水滴铺展,减小表面覆冰面积,同时延迟结冰。
Abstract:
The superhydrophobic coating with micro-nano rough structure and Zn, Ca, P, O, Ce and C elements as the main component was prepared on the surface of galvanized steel by phosphating and sealing treatment combined with surface finishing. The corrosion current density of the superhydrophobic coating is only 9.04×10?7 A/cm 2, which can withstand the corrosion of neutral solution and acid and alkaline solution for a long time, and shows better corrosion resistance than galvanized steel. The superhydrophobic coating can also achieve delayed icing effect and shows delayed freezing performance. The superhydrophobic coating with micro-nano rough structure and low surface energy can be formed on the surface of galvanized steel through composite surface treatment, which effectively blocks the penetration of corrosive media and reduces the corrosion rate. It can also hinder the spreading of water droplets, reduce the surface icing area, and delay freezing

参考文献/References:

[1].张福志, 王兆丽, 李娜, 等. 中式景观亭, 廊建筑新材料与工艺的应用研究[J]. 科技创新与应用, 2024, 14(14): 78-82.
[2].管勇. 家电用电镀锌钢无铬耐指纹涂层制备与性能研究[D]. 沈阳: 中国科学院金属研究所, 2012.
[3].闫宏飞, 包宁, 姜锐. 桥梁缆索用热镀锌钢丝盐雾条件下腐蚀防护的试验研究[J]. 全面腐蚀控制, 2023, 37(2): 61-64.
[4].Saravanan P, Srikanth S. Post treatment of hot dip galvanized steel sheet-chromating, phosphating and other alternative passivation technologies[J]. Journal of Materials Sciences and Applications, 2019, 3: 1-22.
[5].Lee M H, Kim Y W, Lim K M, et al. Electrochemical evaluation of zinc and magnesium alloy coatings deposited on electrogalvanized steel by PVD[J]. Transactions of Nonferrous Metals Society of China, 2013(23): 876-880.
[6].Lin B L, Lu J T, Li Y C. Growth mechanism of composite coatings obtained by phosphating and cerium nitrate post-sealing on galvanized steel[J]. The Chinese Journal of Nonferrous Metals, 2014, 24(4): 1008-1013.
[7].陈耀峰, 邵文鹏, 赵广宾, 等. 金属基体表面超疏水涂层材料的制备及应用研究进展[J]. 材料研究与应用, 2024, 18(1): 106-116.
[8].尤航, 彭毅, 杨冲, 等. 金属超疏水涂层制备及其耐腐蚀性能研究进展[J]. 中国有色金属学报, 2024, 34(3): 703-724.
[9].Wu J, Zhao Y, Li S P, et al. A composite super-hydrophobic coating on M2052 alloy exhibiting corrosion resistance in the marine environment[J]. Transactions of the Indian Institute of Metals, 2024, 77: 2303-2312.
[10].Fang X M, Zhu Q Y, Liu Y D, et al. Preparation of cerium myristate (super) hydrophobic coating by one-step electrodeposition and its protective properties on aluminum alloys[J]. Applied Physics A, 2024, 130: 252.
[11].林碧兰, 卢锦堂, 李月婵. 镀锌层表面磷化/硝酸铈封闭后处理复合膜的生长机理[J]. 中国有色金属学报, 2014, 24(4): 1008-1013.
[12].凌付平. 植酸及铈盐溶液封闭对铝锂合金阳极氧化膜性能的影响[J]. 电镀与精饰, 2023, 45(3): 32-38.
[13].郝晓茹, 张羽, 谢军, 等. 硬脂酸改性三氧化二铝表面润湿性的特性分析[J]. 表面技术, 2023, 52(6): 400-409.
[14].Yu Y H, Dong Y H, Ning H L, et al. A robust superhydrophobic coating with multi-dimensional micro-nano structure on 5052 aluminum alloy[J]. Surface & Coatings Technology, 2023, 465: 129564.
[15].Xu K, Shen W R, Yang S, et al. Laser-enhanced electrodeposition preparation technology of superhydrophobic micro-nano structure coating[J]. Colloids and Surfaces, A. Physicochemical and Engineering Aspects, 2023, 657: 130507.
[16].赵欣, 黄成超, 李梦, 等. 微纳超疏水钛合金表面的制备及其性能研究[J]. 表面技术, 2023, 52(3): 360-369.
[17].刘天, 孙杰, 宋佳, 等. NiCrAl-NiC封严涂层在盐雾环境下的腐蚀行为研究[J]. 表面技术, 2023, 52(1): 206-213.
[18].郭强, 赵巍, 张冲. 热喷涂高铝含量Zn-Al合金涂层热带岛礁大气环境腐蚀行为研究[J]. 装备环境工程, 2024, 21(3): 129-138.
[19].Shetty A R, Hegde A C. Effect of limiting current density on corrosion performance of Ni-Mo, Ni-Cd and Ni-Mo-Cd alloy coatings[J]. Chemical Papers, 2023, 77: 4399-4407.
[20].Qi C H, Lei X L, Zhou B, et al. Temperature regulation of the contact angle of water droplets on the solid surfaces[J]. The Journal of Chemical Physics, 2019, 150(23): 234703.
[21].胡丽娜, 杜一枝, 董立婷, 等. TiO2粒径对TiO2/聚脲超疏水涂层机械稳定性和防覆冰性能的影响研究[J]. 表面技术, 2024, 53(12): 240-251.

相似文献/References:

[1]桂根生*.车用镀锌钢多维腐蚀分析与评估应用研究[J].电镀与精饰,2021,(12):23.[doi:10.3969/j.issn.1001-3849.2021.12.005]
 GUI Gensheng*.Application Research on Multi-dimensional Corrosion Analysis and Evaluation of Galvanized Steel for Automobile[J].Plating & Finishing,2021,(08):23.[doi:10.3969/j.issn.1001-3849.2021.12.005]
[2]边美华,彭家宁,何雨茵,等.doi: 10.3969/j.issn.1001-3849.2025.02.008输电杆塔材料镀锌钢层耐腐蚀性的快速评价探究[J].电镀与精饰,2025,(02):54.
 Bian Meihua,Peng Jianing*,He Yuyin,et al.A rapid evaluation method for corrosion resistance of galvanized steel layer for transmission tower materials[J].Plating & Finishing,2025,(08):54.
[3]王宗江,何 成,阿依古扎力?阿肯江,等.doi: 10.3969/j.issn.1001-3849.2026.03.013镀锌钢和Q235钢在高氯盐环境中腐蚀行为对比[J].电镀与精饰,2026,(03):100.
 WANG Zongjiang,HE Cheng,AYGUZALI Arkanjiang,et al.Comparaison of corrosion behavior of calvanized steel and Q235 steel in high chloride environment[J].Plating & Finishing,2026,(08):100.

更新日期/Last Update: 2025-08-11