参考文献/References:
[1].伍俐, 付天琳, 于晓华, 等. 工业纯钛的阳极氧化特性及其抗腐蚀性能研究[J]. 热加工工艺, 2017, 46(4): 161-164, 167.
[2].彭西洋, 李雪峰. 钛合金在汽车工业中的应用现状及前景展望[J]. 汽车工艺师, 2023(4): 56-59.
[3].訾群. 钛合金研究新进展及应用现状[J]. 钛工业进展, 2008(2): 23-27.
[4].Zheng H M, Xu L, Jiao Y, et al. Fabrication and surface characterization of titanium dioxide nanotubes on titanium implants[J]. Frontiers in Materials, 2023, 10: 1325997.
[5].Otadi M, Borhani E, Faghihi S. Combined bulk nanostru-cturing and surface modifications of titanium substrate for improved corrosion behavior[J]. Surface and Coatings Technology, 2024, 493(2): 131229-131229.
[6].盛利. 钛材在新材料领域的新应用[J]. 中国有色金属, 2017(18): 35.
[7].黄海广, 肖寒, 熊汉城, 等. 钛材低成本生产技术的开发和应用[J]. 云南冶金, 2020, 49(6): 59-67.
[8].Ge M Z, Cao C Y, Huang J Y, et al. Synthesis, modification, and photo/photoelectrocatalytic degradation applications of TiO2 nanotube arrays: a review[J]. Nanotechnology Reviews, 2016, 5(1): 75-112.
[9].姜超平, 孙飞娟, 邢亚龙. 钛合金阳极氧化的研究进展[J]. 热加工工艺, 2018, 47(16): 7-12.
[10].邢俊恒, 夏正斌, 张燕红, 等. 阳极氧化参数对TiO2薄膜结晶行为影响的研究进展[J]. 化工进展, 2013, 32(3): 592-598.
[11].Renna G, Attolico M A, Moramarco V, et al. The role of peening processes as a pre‐treatment to anodizing on fatigue behavior of aircraft aluminum alloy[J]. Fatigue & Fracture of Engineering Materials & Structures, 2024, 47(4): 1312-1330.
[12].Ye Y Y, Zou Q, Xiao Y N, et al. Effect of interface pretreatment of Al alloy on bonding strength of the laser joined Al/CFRTP butt joint[J]. Micromachines, 2021, 12(2): 179.
[13].苏奥, 苏运娟. Ti-6Al-4V钛合金环保型阳极氧化及封闭处理研究[J]. 电镀与精饰, 2024, 46(3): 66-74.
[14].王倩, 何代华, 刘平, 等. 阳极氧化电解质的组分对钛基体和表面涂层的影响[J]. 材料研究学报, 2018, 32(4): 301-308.
[15].Asoh H, Fukumoto S, Shishido K, et al. Anodization of aluminum in a sodium hydroxide solution: effect of pH on chemical dissolution[J]. Journal of the Electrochemical Society, 2024, 171(12): 123504.
[16].Avalos-Hernández E E, Hernández-Torres J, Zamora-Peredo L, et al. Effect of temperature and incorporation of Cr on the microstructure and hardness of titanium anodized with HCl and glycerol[J]. Surface Review and Letters, 2023, 30(12): 2350088.
[17].Xie C Y, Chen Y S, Liu X L, et al. Effect of voltage and time on microstructure and corrosion resistance of anodic oxidation film on Al-5.5Zn-0.03In-1Mg-0.03Ti-0.08Sn alloy[J]. Journal of Alloys and Compounds, 2024, 1009: 176740.
[18].Pham V H, Duc D M, Hung N D, et al. Influence of current density on the morphology and structure of silver nanoparti-cles on anodized titanium for biomedical implant applica-tions[J]. Key Engineering Materials, 2024, 1002: 55-62.
[19].Su K X, Zhang J W, Cui G D, et al. Effects of sealing and prior shot peening treatments on fatigue behavior of sulphuric acid anodic oxidation coated 6082-T6 aluminium alloy[J]. International Journal of Fatigue, 2024, 183: 108251.
[20].Sapoletova N A, Kushnir S E, Ulyanov A N, et al. Effect of post-treatment on photocatalyt-ic activity of anodic titania photonic crystals[J]. Optical Materials, 2023, 144: 114350.
[21].Choi Y, Jeong C. Investigating the influence of pore-widening time control in electrochemical anodization for the formation of hybrid titanium nanostructures with enhanced superhydrophobicity for improved corrosion resistance efficiency[J]. Electrochimica Acta, 2024, 492: 144380.
[22].Aida S, Stefan R, Zinonas E, et al. Predictability and outcome of titanium color after different surface modifications and anodic oxidation[J]. Dental Materials Journal, 2022, 41(6): 930-936.
[23].徐照英, 张腾飞, 苏永要, 等. 钛合金表面阳极氧化着色及摩擦学特性研究[J]. 真空科学与技术学报, 2020, 40(8): 734-740.
[24].Wu L K, Bao Y T, Jiang M Y, et al. Insights into the surface pretreatment on the oxidation behavior of anodized TiAl alloy[J]. Corrosion Science, 2022, 207: 110571.
[25].李宁波. 医用钛及钛合金表面微—纳尺度生物活性氧化膜的感应加热制备及其生物学行为[D]. 济南: 山东大学, 2018.
[26].王志文, 刁瑞佳, 付天林, 等. TA2表面阳极氧化膜机械研磨调控技术及耐腐蚀行为[J]. 材料热处理学报, 2018, 39(5): 100-107.
[27].Sowa M, Greń K, Kukharenko A I, et al. Influence of electropolishing and anodic oxidation on morphology, chemical composition and corrosion resistance of niobium[J]. Materials Science and Engineering: C, 2014, 42: 529-537.
[28].Li W S, Zhang S Q, Li F. Effect of chemical polishing on the formation of TiO2 nanotube arrays using Ti mesh as a raw material[J]. Nanomaterials, 2024, 14(23): 1893.
[29].Wang Z W, Diao R J, Yuan Z T, et al. Surface mechanical attrition treatment and corrosion resistance behavior of TA2 anodic oxide film[J]. International Journal of Electrochemical Science, 2018, 13(5): 4411-4423.
[30].李玉海, 万智来, 蒋国瑜, 等. TA2纯钛材阳极氧化着色工艺[J]. 材料保护, 2011, 44(4): 38-40.
[31].超敏, 肖胜辉, 熊辉, 等. 钛合金阳极氧化工艺过程及其应用态势[J]. 能源研究与管理, 2012(2): 52-55.
[32].郑志军, 何蕊, 陈均焕, 等. 纯钛表面超疏水性着色膜的制备及性能[J]. 中国表面工程, 2020, 33(3): 61-70.
[33].Jiang Z L, Dai X, Norby T, et al. Investigation of pitting resistance of titanium based on a modified point defect model[J]. Corrosion Science, 2010, 53(2): 815-821.
[34].辛富生, 陶麒鹦, 田汉清, 等. 预氧化对于HDH钛粉钝化性能的影响[J]. 中国有色金属学报, 2022, 32(4): 940-950.
[35].杜青. 喷砂酸蚀(SLA)钛表面生物活化及性能表征[D]. 哈尔滨: 哈尔滨工业大学, 2016.
[36].王雨晨. 多孔钛材的表面改性对其耐蚀性及导电性的影响[D]. 北京: 北京化工大学, 2024.
[37].付天琳, 梅长云, 陈飞帆, 等. 表面纳米化对纯钛阳极氧化膜组织及特性的影响[J]. 稀有金属材料与工程, 2022, 51(3): 835-842.
[38].孔玢, 李丽, 刘正乔, 等. 工业纯钛在硫酸中的腐蚀行为及其机理研究[J]. 钛工业进展, 2022, 39(2): 18-23.
[39].Li X, Wang L, Fan L, et al. Understanding the effect of fluoride on corrosion behavior of pure titanium in different acids[J]. Corrosion Science, 2021, 192: 109812.