Liu Zhiying,Li Mingmao*,Yin Ningkang,et al.Suggestions and standardization suggestions for electrolytic copper foil in lithium-ion battery[J].Plating & Finishing,2024,(10):73-82.
锂离子电池用电解铜箔产业趋势和标准化建议
- Title:
- Suggestions and standardization suggestions for electrolytic copper foil in lithium-ion battery
- Keywords:
- lithium-ion battery; electrolytic copper foil; lithium battery and copper foil; industrial trend; standardization suggestion
- 分类号:
- TG146.1
- 文献标志码:
- A
- 摘要:
- 随着低碳政策的持续实施,作为新能源材料的锂离子电池用电解铜箔(简称锂电铜箔)产能产量呈井喷式发展,国内锂电铜箔制造技术迅速提升至全球领先水平,飞速的发展也带来一系列问题。梳理了国内锂电铜箔的发展历程、厚度变化趋势、装备国产化情况、近七年产能产量,提出了锂电铜箔行业下一步主攻方向和建议,提出了锂电铜箔产品、方法标准和产品碳足迹标准存在的问题及制/修订建议。
- Abstract:
- With the continuous implementation of low-carbon policies, as a new energy material, the production capacity of electrolytic copper foil for lithium-ion batteries (hereinafter referred to as lithium battery and copper foil) has been blowout development, and the domestic lithium copper foil manufacturing technology has rapidly improved to the world’s leading level. However, the rapid development also brings a series of problems. The development process of domestic lithium battery and copper foil in China, the trend of thickness changes, the domestic production of equipment, the production energy and production in the past seven years are reviewed, and the next main attack direction and suggestions of the lithium battery and copper foil industry are proposed, and the problems and revision suggestions of lithium copper foil products, method standards and product carbon footprint standards are also put forward
参考文献/References:
[1].人民网. 产销同比双增 中国一汽实现首季开门红[EB/OL]. http://finance.people.com.cn/GB/n1/2024/0403/ c1004-40209570.html, 2024-04-03/2024-04-09.
[2].高工锂电. 新能源车平均带电量提升: BEV58.5度, PHEV28.8度[EB/OL]. https://mp.weixin.qq.com/s/Mu XdGslOoE66sVCfR4FzOw, 2024-04-04/2024-04-09.
[3].李映泉. 铜箔紧缺涨势凶猛 爆发式扩产难解近渴[N]. 证券时报, 2021-07-02 (A09).
[4].黄洁. 铜箔的生产技术及发展趋向[J]. 铜业工程, 2003(2): 83-84.
[5].金荣涛. 电解铜箔产业发展趋势[J]. 印制电路信息, 2003(2): 22-24, 31.
[6].思瀚产业研究院. 锂电铜箔行业情况及产业链上下游分析[EB/OL]. https://baijiahao.baidu.com/s?id=17738279 20434602347&wfr=spider&for=pc, 2023-08-10/2024-03-16.
[7].万新领, 高元亨, 刘龙富. 一种用于生产铜箔的高效溶铜罐: 中国, CN202220185459.3[P]. 2022-08-12.
[8].杨声鸿, 刘晓燕, 杨剑文, 等. 一种电解铜箔自动溶铜装置: 中国, CN202211432522.X [P]. 2023-07-07.
[9].黄练彬, 杨剑文, 杨雨平, 等. 一种具有搅拌铲料功能的铜箔生产用溶铜罐: 中国, CN202210157014.9 [P]. 2023-04-25.
[10].叶敬敏, 王俊锋, 刘少华, 等. 用于6微米铜箔生产的溶铜罐: 中国, CN201910527592.5[P]. 2020-09-18.
[11].张贵斌, 郑惠军, 周启伦, 等. 一种生箔机阳极槽: 中国, CN201720138247.9 [P]. 2017-07-07.
[12].万新领, 高元亨, 关灿球. 一种防止铜箔撕边的阳极板: 中国, CN201921863618.5 [P]. 2020-06-30.
[13].孙凤岭. 一种搭焊与锻打变形复合成形方法: 中国, CN202111185660.8 [P]. 2024-04-26.
[14].沈楚, 冯庆, 王思琦, 等. 一种超大幅宽旋压阴极辊制造方法: 中国, CN202111390451.7 [P]. 2023-09-19.
[15].王超, 冯庆, 何秀玲, 等. 一种电解铜箔用无缝阴极辊钛筒的制造方法: 中国, CN202210742263.4 [P]. 2023-08-04.
[16].苗东, 葛晓林, 冯庆, 等. 一种大规格阴极辊及制造方法: 中国, CN202210528775.0 [P]. 2023-04-11.
[17].李博, 冯庆, 苗东, 等. 一种导电能力强的阴极辊加工装置及其加工流程: 中国, CN202210015829.3 [P]. 2023-03-14.
[18].张乐, 冯庆, 王思琦, 等. 一种用于生产高强极薄铜箔的大幅宽阴极辊: 中国, CN202111521532.6 [P]. 2022-10-18.
[19].杨勃, 冯庆, 李博, 等. 一种更换方便低成本的阴极辊: 中国, CN202111617234.7 [P]. 2022-08-12.
[20].张乐, 冯庆, 沈楚, 等. 一种大直径钛合金筒形件的冷旋压成形方法: 中国, CN202111421906.7 [P]. 2023-04-14.
[21].李建伟, 廖平元, 刘少华, 等. 电解铜箔生产甚低轮廓铜箔用阴极辊的研磨方法: 中国, CN201410259970.3 [P]. 2017-03-01.
[22].景冬建, 松田光也, 陈贤生. 一种阴极辊表面研磨装置: 中国, CN202111080195.1 [P]. 2022-06-24.
[23].凌超军, 廖平元, 刘少华, 等. 一种铜箔生产用阴极辊在线抛光装置: 中国, CN202210518982.8 [P]. 2023-07-28.
[24].王凤梅, 杨剑文, 杨雨平, 等. 一种电解铜箔抛光辊自动清理设备: 中国, CN202211342262.7 [P]. 2023-05-23.
[25].周启伦. 一种制造5微米高抗拉铜箔用的添加剂及工艺: 中国, CN201811101179.4 [P]. 2018-12-11.
[26].万新领, 高元亨, 刘龙富. 一种铜箔生产中电解液的过滤装置: 中国, CN202220356076.8 [P]. 2022-06-14.
[27].万新领, 高元亨, 罗志艺, 等. 电解铜箔生箔机电解槽用进液调节阀: 中国, CN202221302606.7 [P]. 2022-11-15.
[28].彭颂, 叶铭, 廖平元, 等. 一种电解铜箔设备精密配液装置: 中国, CN202111012119.7 [P]. 2022-05-13.
[29].万新领, 高元亨, 聂谷明. 一种新型锂电铜箔烘烤箱装置: 中国, CN202223043994.4 [P]. 2023-02-28.
[30].林炼钦, 潘文俊, 黄集贤, 等. 基于耳料的电解铜箔翘曲测试机具及测试方法: 中国, CN202210269373.3 [P]. 2022-11-01.
[31].郭丽平, 郑衍年, 刘少华, 等. 一种动力电池用电解铜箔翘曲连续化测试方法及设备: 中国, CN202210224457.5 [P]. 2022-09-27.
[32].林伟民, 郭志航, 邹子萍, 等. 一种具有铜箔端部翘曲在线检测处理装置的生产线: 中国, CN202110214302.9 [P]. 2021-09-14.
[33].曾尚南, 杨剑文, 杨雨平, 等. 一种电解铜箔降低翘曲量处理设备以及处理方法: 中国, CN202210355814.1 [P]. 2022-12-02.
[34].郑衍年, 郭丽平, 刘少华, 等. 一种端部型电热的电解铜箔防翘曲设备及其工作方法: 中国, CN202210434290.5 [P]. 2022-11-29.
[35].杨弘, 洪远程, 杨扬, 等. 一种极薄铜箔的制造方法及其生产设备: 中国, CN202210197401.5 [P]. 2022-10-14.
[36].杨雨平, 陈优昌, 李志华, 等. 一种具有撕边在线收卷装置的生箔机: 中国, CN202111006243.2 [P]. 2022-02-11.
[37].万新领, 高元亨, 罗志艺, 等. 一种张力分散均匀的辊类装置: 中国, CN201921723046.0 [P]. 2020-05-29.
[38].万新领, 高元亨, 罗志艺, 等. 一种带自动调节辊的铜箔收卷装置: 中国, CN202220354985.8 [P]. 2022-06-07.
[39].周启伦, 万新领. 一种生箔收卷压辊装置: 中国, CN201821639055.7 [P]. 2019-05-24.
[40].王爱军, 廖平元, 杨剑文, 等. 一种铜箔厚度均匀性处理方法、铜箔表面处理方法: 中国, CN202010568715.2 [P]. 2021-01-19.
[41].郭丽平, 廖平元, 刘少华, 等. 一种电解铜箔厚度均匀性自动化测定系统: 中国, CN201911303308.2 [P]. 2020-08-11.
[42].温欢元, 杨剑文, 杨雨平, 等. 基于电解电流的离散化铜箔厚度监测方法以及监测系统: 中国, CN202210641000.4 [P]. 2023-05-12.
[43].杨艳球, 郭志航, 郑衍年, 等. 一种电解铜箔纵向尺度均匀性测量方法、系统、生箔机: 中国, CN202210025712.3[P]. 2023-05-02.
[44].黄勇, 廖平元, 温佳栋, 等. 一种铜箔生产方法以及铜箔厚度检测方法、存储介质: 中国, CN202210642314.6 [P]. 2023-03-21.
[45].万新领, 高元亨, 胡月清. 一种分切在线厚度检测装置: 中国, CN201821597711.1 [P]. 2019-04-19.
[46].万新领, 高元亨, 刘丕冲. 一种分切表面缺陷在线检测装置: 中国, CN201821599943.0 [P]. 2019-04-19.
[47].郭丽平, 廖平元, 刘少华, 等. 用于检测铜箔渗透针孔的硫酸自动涂刷设备: 中国, CN201810633847.1 [P]. 2023-08-08.
[48].邹子萍, 郭丽平, 刘少华, 等. 一种电解铜箔针孔检测标记系统: 中国, CN202210240367.5 [P]. 2023-06-06.
[49].廖平元, 杨剑文, 李永根, 等. 一种铜箔表面色差检测与修复装置: 中国, CN201810047456.1 [P]. 2023-09-05.
[50].王俊锋, 王崇华, 刘焕添, 等. 一种铜箔表面色差修复的处理方法: 中国, CN201810047420.3 [P]. 2023-06-23.
[51].杨苑, 王崇华, 廖平元, 等. 一种防止4.5μm铜箔发白的生产方法: 中国, CN202210151131.4 [P]. 2022-09-27.
[52].王崇华, 张小玲, 廖平元, 等. 一种波浪纹检测纠正设备: 中国, CN201620505294.8 [P]. 2016-10-12.
[53].李建国, 庄如珍, 廖平元, 等. 一种铜箔表面酸雾点控制装置: 中国, CN201820513368.1 [P]. 2018-11-16.
[54].温丙台, 曾嘉文, 谢佳博, 等. 一种多工位硬度检测装置: 中国, CN202320375877.3 [P]. 2023-07-28.
[55].曾嘉文, 温丙台, 谢佳博, 等. 一种铜箔力学性能检测用夹持装置: 中国, CN202222904757.6 [P]. 2023-05-23.
[56].凌超军, 廖平元, 刘少华, 等. 一种铜箔抗拉延伸率在线抽样检测装置: 中国, CN202110881847.5 [P]. 2021-12-28.
[57].刘晓燕, 王洪杰, 庄伟雄, 等. 一种铜箔延展性能测试装置及工艺: 中国, CN202211011084.X [P]. 2023-03-14.
[58].温丙台, 洪远程, 郑衍年, 等. 一种铜箔生产用抗拉强度检测装置: 中国, CN202222158166.9 [P]. 2023-01-03.
[59].张小玲, 陈优昌, 邹子萍, 等. 一种锂离子电池用铜箔铜粉粒度检测装置: 中国, CN201520212066.7 [P]. 2015-07-15.
[60].庄如珍, 李建国, 陈优昌, 等. 一种铜箔铜粉清除装置及使用方法: 中国, CN201610237522.2 [P]. 2017-12-08.
[61].高鹏, 王晓远. 轴向磁场复合PCB定子有铁心永磁同步电机: 中国, CN202010100324.8[P]. 2022-07-12.
[62].刘若曦. 铜箔行业的强者之争[J]. 中国有色金属, 2015(14): 58-59.
[63].龚永林. 中国早期印制电路板生产技术回顾(1)[J]. 印制电路信息, 2023, 31(3): 4-10.
[64].曹伍. 铜箔成为中科英华第二大主业[N]. 中国有色金属报, 2006-04-20 (006).
[65].陈平华. 电解铜箔市场研究报告[J]. 世界有色金属, 2005,(5): 19-27.
[66].诺德股份. 喜讯: 诺德股份获“最具成长力企业二十强”殊荣[EB/OL]. https://mp.weixin.qq.com/s/kOOoSGXj4Q 63-12K4fYaTw, 2024-05-30/2024-06-01.
[67].樊娅楠. 用实力书写炼铜成纸的奇迹[N]. 西宁晚报, 2023-08-25 (A09).
[68].财是. 嘉元科技专题研究报告: 铜箔技术迭代叠加产能释放,迎来量利双升[EB/OL]. https://baijiahao.baidu.com/ s?id=1701057664370301510&wfr=spider&for=pc, 2021-05-29/2024-03-16.
[69].东方财富网. 嘉元科技: 已向国内头部锂电池厂商批量供应4.5 μm 铜箔产品[EB/OL]. https://finance.eastmoney. com/a/202011091694355325.html, 2020-11-09/2024-03-16.
[70].江铜铜箔首卷万米4.0 μm极薄锂电铜箔顺利下卷[J]. 有色金属材料与工程, 2022, 43(3): 62.
[71].大河网. 这些豫企相当潮丨灵宝铜箔何以领跑[EB/OL]. https://baijiahao.baidu.com/s?id=1782791469699626498&wfr=spider&for=pc, 2023-11-17/2024-03-16.
[72].米绪军, 娄花芬, 解浩峰, 等. 我国先进铜基材料发展战略研究[J]. 中国工程科学, 2023, 25(1): 8.
[73].Murphy D, Broadhead J, Steele B. Materials for advanced batteries[M]. New York: Plenum Press, 1980.
[74].Nishi Y. The development of lithium ion secondary batteries[J]. Chemical Record, 2001, 1(5): 406-413.
[75].Nishi Yoshio. Lithium ion secondary hatteries: Past 10 years and the future [J]. Journal of Power Sources, 2001, 100: 101.
[76].Chu H-C, Tuan H-Y. High-performance lithium-ion batteries with 1.5 μm thin copper nanowire foil as a current collector [J]. Journal of Power Sources, 2017, 346: 40-48.
[77].Nagpure S C, Downing R G, Bhushan B, et al. Discovery of lithium in copper current collectors used in batteries[J]. Scripta Materialia, 2012, 67: 669-672.
[78].超华科技: 被忽视的锂电池核心材料供应商[J]. 股市动态分析, 2016(24): 51.
[79].中国有色金属加工工业协会. 高端市场需求迫切 锂电铜箔超薄化进程加速[EB/OL]. https://www.cnfa.net.cn/ news/show-2219.aspx, 2019-12-23/2024-05-23.
[80].财是. 嘉元科技专题研究报告: 铜箔技术迭代叠加产能释放, 迎来量利双升[EB/OL]. https://baijiahao.baidu. com/s?id=1701057664370301510&wfr=spider&for=pc, 2021-05-29/2024-03-16.
[81].任利娜, 侯智敏, 牛靖, 等. 电解铜箔用阴极辊的研究进展及发展趋势[J]. 精密成形工程, 2020, 12(2): 84-92.
[82].潇湘晨报. 这项“西安科技”填补国内空白!国内首个3米直径新能源锂电铜箔核心装备阴极辊发布面市[EB/OL]. https://baijiahao.baidu.com/s?id=1744764249594481712&wfr=spider&for=pc, 2022-09-23/2024-03-16.
[83].西安新闻网. 新能源锂电铜箔核心装备大直径3.6米阴极辊填补国内空白 西安泰金新能彰显“中国智造”力量[EB/OL]. https://www.xiancn.com/content/2023-04/02/ content_6708151.htm, 2023-04-02/2024-03-16.
[84].知乎. 新能源锂电铜箔装备新纪录!国内最大直径3.6米阴极辊成功下线交付客户[EB/OL]. https://zhuanlan. zhihu.com/p/673433256, 2023-12-15/2024-03-16.
[85].邱熙然, 朱逸慧. 三门峡: 勠力“铜”心厚积“箔”发[J]. 中国有色金属, 2021(11): 31-35.
[86].章新亮, 刘志英, 饶锦武, 等. 国内铜工业进展与江西铜产品现状[J]. 世界有色金属, 2019(18): 239-242.
[87].王乔琪. 海亮股份拟斥资59亿海外扩产电解铜箔[N]. 上海证券报, 2023-02-28 (005).
[88].中华人民共和国工业和信息化部. SJ/T 11483-2014 锂离子电池用电解铜箔[S]. 北京: 中国电子技术标准化研究院, 2014.
[89].徐龙, 徐辉, 何桂青, 等. 改善4.5μm铜箔无法连续收卷问题的添加剂工艺[J]. 安徽科技, 2021(10): 47-50.
[90].李民, 陶炳贞, 杨孝坤. 一种4.5μm极薄电解铜箔的制备装置及其制备工艺: 中国, CN202010032482.4 [P]. 2022-02-18.
[91].马校彬, 潘建锋, 马志华, 等. 一种无铬环保型超薄锂电铜箔及其制备工艺: 中国, CN202211583067.3 [P]. 2023-07-04.
[92].操声跃, 张红亮, 何桂青, 等. 一种锂离子电池用4.5μm电解铜箔、制备方法及添加剂: 中国, CN201910871243.5 [P]. 2021-07-06.
[93].王俊锋, 钟孟捷, 叶敬敏, 等. 一种普强型锂离子电池用极薄电解铜箔的制备方法: 中国, CN202010053832.5 [P]. 2021-07-16.
[94].王俊锋, 刘晓燕, 郭志航, 等. 一种高抗拉强度锂离子电池用极薄电解铜箔的制备方法: 中国, CN202010053840.X [P]. 2021-06-18.
[95].叶铭, 廖平元, 刘少华, 等. 一种超薄铜箔及其制备方法: 中国, CN202110161499.4 [P]. 2021-12-28.
[96].彭颂, 廖平元, 叶铭, 等. 一种电解铜箔及其制备方法: 中国, CN202110161468.9 [P]. 2021-06-18.
[97].刘少华, 王俊锋, 叶敬敏, 等. 超薄电解铜箔的制造方法: 中国, CN200810220571.0 [P]. 2011-07-13.
[98].国家技术监督局. GB/T 5230—1995 电解铜箔[S]. 北京: 中国标准出版社, 1995.
[99].中华人民共和国国家质量监督检验检疫总局, 中国国家标准化管理委员会. GB/T 22638.4—2008 铝箔试验方法 第4部分: 表面润湿张力的测定[S]. 北京: 中国标准出版社, 2009.
[100].国家市场监督管理总局, 国家标准化管理委员会. GB/T 5230—2020 印制板用电解铜箔[S]. 北京: 中国标准出版社, 2020.
[101].中华人民共和国国家质量监督检验检疫总局, 中国国家标准化管理委员会. GB/T 6462—2005 金属和氧化物覆盖层 厚度测量 显微镜法[S]. 北京: 中国标准出版社, 2005.
[102].中华人民共和国国家质量监督检验检疫总局, 中国国家标准化管理委员会. GB/T 5121.1—2008 铜及铜合金化学分析方法 第1部分: 铜含量的测定[S]. 北京: 中国标准出版社, 2008.
[103].中华人民共和国国家质量监督检验检疫总局, 中国国家标准化管理委员会. GB/T 22638.4—2016 铝箔试验方法 第4部分: 表面润湿张力的测定[S]. 北京: 中国标准出版社, 2016.
[104].中华人民共和国国家质量监督检验检疫总局, 中国国家标准化管理委员会. GB/T 29847—2013 印制板用铜箔试验方法[S]. 北京: 中国标准出版社, 2013.
相似文献/References:
[1]程庆,李宁,潘钦敏*,等.电解铜箔添加剂的研究进展及应用现状[J].电镀与精饰,2022,(12):69.[doi:10.3969/j.issn.1001-3849.2022.12.010]
CHENG Qing,LI Ning,PAN Qinmin*,et al.Research Progress and Application Status of Electrolytic Copper Foil Additives[J].Plating & Finishing,2022,(10):69.[doi:10.3969/j.issn.1001-3849.2022.12.010]
[2]陈媛媛,徐常龙,陈修栋 *,等.Co3O4纳米空心球电极的制备及其储锂性能[J].电镀与精饰,2023,(9):95.[doi:10.3969/j.issn.1001-3849.2023.09.015]
Chen Yuanyuan,Xu Changlong,Chen Xiudong *,et al.Preparation and lithium storage performance of Co 3 O 4 nanometer hollow sphere electrode[J].Plating & Finishing,2023,(10):95.[doi:10.3969/j.issn.1001-3849.2023.09.015]
[3]张锦园,张菁丽,白忠波,等.电解铜箔用钛阳极涂层的研究现状[J].电镀与精饰,2023,(12):95.[doi:doi : 10.3969/j.issn.1001-3849.2023.12.014]
Zhang Jinyuan,Zhang Jingli,Bai Zhongbo,et al.Research status of titanium anode coating for electrolytic copper foil[J].Plating & Finishing,2023,(10):95.[doi:doi : 10.3969/j.issn.1001-3849.2023.12.014]
[4]代超熠,唐先忠,何 为,等.电解铜箔添加剂的研究进展[J].电镀与精饰,2024,(2):79.[doi:10.3969/j.issn.1001-3849.2024.02.011]
Tang Yao,hen Yuanming *.Research progress of electrolytic copper foil additives[J].Plating & Finishing,2024,(10):79.[doi:10.3969/j.issn.1001-3849.2024.02.011]
[5]彭雪嵩,由宏伟,李兰晨,等.粗化工艺对电解铜箔抗剥离强度和劣化率的影响[J].电镀与精饰,2024,(3):95.[doi:10.3969/j.issn.1001-3849.2024.03.014]
Peng Xuesong,You Hongwei,Li Lanchen,et al.The influence of coarsening process on the anti-peeling strength and degradation rate of electrolytic copper foil?/html>[J].Plating & Finishing,2024,(10):95.[doi:10.3969/j.issn.1001-3849.2024.03.014]
[6]樊斌锋,王丽娜*,王庆福,等.新型添加剂提高锂电铜箔高温延伸率的研究[J].电镀与精饰,2024,(3):108.[doi:10.3969/j.issn.1001-3849.2024.03.016]
Fan Binfeng,Wang Lina*,Wang Qingfu,et al.Study on improving the elongation of lithium copper foil with new additives at high temperature[J].Plating & Finishing,2024,(10):108.[doi:10.3969/j.issn.1001-3849.2024.03.016]
[7]张锦园,张 杰,白忠波,等.硫酸钛-钨酸钠复合添加剂对电解铜箔后处理形貌及抗剥离强度的影响[J].电镀与精饰,2024,(5):101.[doi:10.3969/j.issn.1001-3849.2024.05.014]
Zhang Jinyuan,Zhang Jie,Bai Zhongbo,et al.Effect of titanium sulfate and sodium tungstate composite additive on morphology and performance of electrolytic copper foil posttreatment?/html>[J].Plating & Finishing,2024,(10):101.[doi:10.3969/j.issn.1001-3849.2024.05.014]
[8]樊斌锋,程润润*,王庆福,等.添加剂HP在复合添加剂中对电解铜箔组织性能的影响[J].电镀与精饰,2024,(10):28.
Fan Binfeng,Cheng Runrun*,Wang Qingfu,et al.Effect of additive HP in combination additives on the organizational properties of electrolytic copper foils[J].Plating & Finishing,2024,(10):28.
[9]涂敏,陈息坤.还原氧化石墨烯合成及在锂离子电池中应用[J].电镀与精饰,2024,(12):40.
Tu Min *,Chen Xikun.Synthesis of SnS2/reduced graphene oxide and its application in lithium ion batteries[J].Plating & Finishing,2024,(10):40.
[10]王庆福,王丽娜,樊斌锋,等.doi: 10.3969/j.issn.1001-3849.2025.01.001噻唑及氨基脲衍生物与氯离子作用于电沉积铜的研究[J].电镀与精饰,2025,(01):1.
Wang Qingfu,Wang Lina*,Fan Binfeng,et al.Study on the interaction between thiazole and aminourea derivatives and chloride ions in the electrodeposition of copper[J].Plating & Finishing,2025,(10):1.